MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYLSTAR® AF 218 V25 BLACK 21N PA 66 25% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYLSTAR® AF 218 V25 BLACK 21N is a polyamide 6.6, high flow, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Key Properties: Easy processing; Heat stabilized; Suitable for Mucell®; Good surface aspect

Benefits: This product has enhanced molding behaviors and better surface aspect. It offers an excellent combination between thermal and mechanical properties. This grade is ideal for use in the automotive industry for engine components. This grade is ideal for Mucell® injection molding technology.

Applications: This grade is suitable for all kind of applications in automotive, especially pulley application by giving very low rugosity levels.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183/A
Water Absorption 0.90 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0071 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0085 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPaISO 527 Type 1A
Elongation at Break 2.7 %ISO 527 Type 1A
Tensile Modulus 8800 MPaISO 527 Type 1A
Charpy Impact Unnotched 55.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 285 °CCompression zone
 285 - 290 °CMixing zone
Feed Temperature 270 - 275 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Domo TECHNYLSTAR® AF 219 V30 PA 66 30% Glass Reinforced, Dry
Domo TECHNYLSTAR® AF 218 V30 BLACK 21N PA 66 30% Glass Reinforced, Conditioned
Akro-Plastic Akroloy® PA GF 30 natural (3177) PA 66 + PA 6I/6T Dry, 30% Glass Filled

PSOLVAY867 / 218595

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.