MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Pressure Seal 9809 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9809 is an 80 durometer, high fluorine content, black colored Fluorinated Hydrocarbon elastomer. It is formulated for applications requiring very high chemical resistance, particularly for use in alcohol extended fuels. It exhibits excellent resistance to heat, petroleum based oils, aliphatic and aromatic fuels.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 815 A1-10 B37 B38 EF31 EO78; 4 HK 815 B38 EF31 EO78; 6 HK 815 A1-10 EF31 EO88

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79
 71
@Treatment Temp. 200 °C,
Time 252000 sec
Stauffer Blend 7700
 73
@Treatment Temp. 200 °C,
Time 252000 sec
Service Fluid 101
 75
@Treatment Temp. 23.0 °C,
Time 252000 sec
Gasahol
 75
@Treatment Temp. 23.0 °C,
Time 252000 sec
Toluene
 78
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 78
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3
 79
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 79
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
 79
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 79
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 81
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
 82
@Treatment Temp. 275 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1901 psi
 1216.6 psi
@Treatment Temp. 275 °C,
Time 252000 sec
Heat Aged
 1294.6 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
Gasahol
 1446.7 psi
@Treatment Temp. 200 °C,
Time 252000 sec
Stauffer Blend 7700
 1492.3 psi
@Treatment Temp. 200 °C,
Time 252000 sec
Service Fluid 101
 1589.2 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
Toluene
 1610.1 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3
 1636.8 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 1695.7 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 1756.6 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 1828.8 psi
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
 1904.8 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
Elongation, Ultimate 250 %
 250 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 250 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3
 250 %
@Treatment Temp. 200 °C,
Time 252000 sec
Service Fluid 101
 250 %
@Treatment Temp. 200 °C,
Time 252000 sec
Stauffer Blend 7700
 250 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Gasahol
 250 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Toluene
 260 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 260 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 260 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 260 %
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
 340 %
@Treatment Temp. 275 °C,
Time 252000 sec
Heat Aged
100% Modulus 741 psi
Tear Strength 244 pliDie B
Compression Set 14.5 %
@Treatment Temp. 175 °C,
Time 79200 sec
Plied
 18.4 %
@Treatment Temp. 200 °C,
Time 79200 sec
Plied
 20.3 %
@Treatment Temp. 23.0 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature 19.0 °F
Shrinkage 0.00 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 0.40 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 0.90 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel B
 1.4 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 1.5 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 3.5 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, Toluene
 3.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 6.4 %
@Treatment Temp. 200 °C,
Time 252000 sec
Volume, Service Fluid 100
 7.9 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, Gasahol
 8.1 %
@Treatment Temp. 200 °C,
Time 252000 sec
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL126 / 318336

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.