MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pressure Seal 9809 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9809 is an 80 durometer, high fluorine content, black colored Fluorinated Hydrocarbon elastomer. It is formulated for applications requiring very high chemical resistance, particularly for use in alcohol extended fuels. It exhibits excellent resistance to heat, petroleum based oils, aliphatic and aromatic fuels.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 815 A1-10 B37 B38 EF31 EO78; 4 HK 815 B38 EF31 EO78; 6 HK 815 A1-10 EF31 EO88

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 g/cc1.90 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7979
 71
@Treatment Temp. 200 °C,
Time 252000 sec
71
@Treatment Temp. 392 °F,
Time 70.0 hour
Stauffer Blend 7700
 73
@Treatment Temp. 200 °C,
Time 252000 sec
73
@Treatment Temp. 392 °F,
Time 70.0 hour
Service Fluid 101
 75
@Treatment Temp. 23.0 °C,
Time 252000 sec
75
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Gasahol
 75
@Treatment Temp. 23.0 °C,
Time 252000 sec
75
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Toluene
 78
@Treatment Temp. 150 °C,
Time 252000 sec
78
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
 78
@Treatment Temp. 150 °C,
Time 252000 sec
78
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 79
@Treatment Temp. 23.0 °C,
Time 252000 sec
79
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 79
@Treatment Temp. 100 °C,
Time 252000 sec
79
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 79
@Treatment Temp. 23.0 °C,
Time 252000 sec
79
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 79
@Treatment Temp. 23.0 °C,
Time 252000 sec
79
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 81
@Treatment Temp. 250 °C,
Time 252000 sec
81
@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged
 82
@Treatment Temp. 275 °C,
Time 252000 sec
82
@Treatment Temp. 527 °F,
Time 70.0 hour
Heat Aged
Tensile Strength 13.11 MPa1901 psi
 8.3882 MPa
@Treatment Temp. 275 °C,
Time 252000 sec
1216.6 psi
@Treatment Temp. 527 °F,
Time 70.0 hour
Heat Aged
 8.9260 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1294.6 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Gasahol
 9.9746 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
1446.7 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
Stauffer Blend 7700
 10.289 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
1492.3 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
Service Fluid 101
 10.957 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1589.2 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Toluene
 11.101 MPa
@Treatment Temp. 150 °C,
Time 252000 sec
1610.1 psi
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 11.285 MPa
@Treatment Temp. 150 °C,
Time 252000 sec
1636.8 psi
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
 11.691 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1695.7 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 12.111 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1756.6 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 12.609 MPa
@Treatment Temp. 250 °C,
Time 252000 sec
1828.8 psi
@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged
 13.133 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1904.8 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
Elongation, Ultimate 250 %250 %
 250 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
250 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 250 %
@Treatment Temp. 150 °C,
Time 252000 sec
250 %
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 250 %
@Treatment Temp. 200 °C,
Time 252000 sec
250 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Service Fluid 101
 250 %
@Treatment Temp. 200 °C,
Time 252000 sec
250 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Stauffer Blend 7700
 250 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
250 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Gasahol
 250 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
250 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Toluene
 260 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
260 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 260 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
260 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 260 %
@Treatment Temp. 150 °C,
Time 252000 sec
260 %
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
 260 %
@Treatment Temp. 250 °C,
Time 252000 sec
260 %
@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged
 340 %
@Treatment Temp. 275 °C,
Time 252000 sec
340 %
@Treatment Temp. 527 °F,
Time 70.0 hour
Heat Aged
100% Modulus 5.11 MPa741 psi
Tear Strength 42.8 kN/m244 pliDie B
Compression Set  14.5 %
@Treatment Temp. 175 °C,
Time 79200 sec
14.5 %
@Treatment Temp. 347 °F,
Time 22.0 hour
Plied
 18.4 %
@Treatment Temp. 200 °C,
Time 79200 sec
18.4 %
@Treatment Temp. 392 °F,
Time 22.0 hour
Plied
 20.3 %
@Treatment Temp. 23.0 °C,
Time 79200 sec
20.3 %
@Treatment Temp. 73.4 °F,
Time 22.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -7.22 °C19.0 °F
Shrinkage  0.00 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
0.00 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel A
 0.40 %
@Treatment Temp. 150 °C,
Time 252000 sec
0.40 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 0.90 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
0.90 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel B
 1.4 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
1.4 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel C
 1.5 %
@Treatment Temp. 150 °C,
Time 252000 sec
1.5 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 3.5 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
3.5 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, Toluene
 3.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
3.7 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 6.4 %
@Treatment Temp. 200 °C,
Time 252000 sec
6.4 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Volume, Service Fluid 100
 7.9 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
7.9 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, Gasahol
 8.1 %
@Treatment Temp. 200 °C,
Time 252000 sec
8.1 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL126 / 318336

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.