MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pressure Seal 3717 Nitrile - Butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 3717 is a 70 durometer black colored Buna N elastomer, it is formulated with molybdenum disulfide to provide self lubrication. It exhibits good resistance to aromatic and aliphatic fuels.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 715 B14 B34 EO14; 2 BG 715 B14 B34 EA14 EF11 EF21 EO14; 5 BG 715 A14 B14 B34 EO14
This Compound is RoHS Compliant

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7474
 60
@Treatment Temp. 23.0 °C,
Time 252000 sec
60
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 63
@Treatment Temp. 23.0 °C,
Time 252000 sec
63
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 72
@Treatment Temp. 100 °C,
Time 252000 sec
72
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 74
@Treatment Temp. 23.0 °C,
Time 252000 sec
74
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 79
@Treatment Temp. 100 °C,
Time 252000 sec
79
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 81
@Treatment Temp. 125 °C,
Time 252000 sec
81
@Treatment Temp. 257 °F,
Time 70.0 hour
ASTM Oil #3
 81
@Treatment Temp. 150 °C,
Time 252000 sec
81
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 83
@Treatment Temp. 100 °C,
Time 252000 sec
83
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 86
@Treatment Temp. 125 °C,
Time 252000 sec
86
@Treatment Temp. 257 °F,
Time 70.0 hour
ASTM Oil #1
 86
@Treatment Temp. 100 °C,
Time 252000 sec
86
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 86
@Treatment Temp. 100 °C,
Time 252000 sec
86
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 88
@Treatment Temp. 125 °C,
Time 252000 sec
88
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 88
@Treatment Temp. 125 °C,
Time 252000 sec
88
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
 88
@Treatment Temp. 150 °C,
Time 252000 sec
88
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
Tensile Strength 11.36 MPa1648 psi
 9.3059 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1349.7 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 9.6354 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1397.5 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 11.2149 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
1626.58 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 11.993 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1739.4 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 12.442 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1804.6 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 12.786 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1854.4 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 13.067 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1895.2 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 13.408 MPa
@Treatment Temp. 150 °C,
Time 252000 sec
1944.6 psi
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 14.180 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
2056.7 psi
@Treatment Temp. 257 °F,
Time 70.0 hour
ASTM Oil #3
 14.385 MPa
@Treatment Temp. 150 °C,
Time 252000 sec
2086.4 psi
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
 14.487 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
2101.2 psi
@Treatment Temp. 257 °F,
Time 70.0 hour
ASTM Oil #1
 15.0440 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
2181.95 psi
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 15.0440 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
2181.95 psi
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
Elongation, Ultimate 431 %431 %
 234.9 %
@Treatment Temp. 125 °C,
Time 252000 sec
234.9 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
 234.9 %
@Treatment Temp. 125 °C,
Time 252000 sec
234.9 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 246.96 %
@Treatment Temp. 150 °C,
Time 252000 sec
246.96 %
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 277.13 %
@Treatment Temp. 125 °C,
Time 252000 sec
277.13 %
@Treatment Temp. 257 °F,
Time 70.0 hour
ASTM Oil #3
 309.9 %
@Treatment Temp. 100 °C,
Time 252000 sec
309.9 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged, Test Tube Method
 309.9 %
@Treatment Temp. 100 °C,
Time 252000 sec
309.9 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 343.1 %
@Treatment Temp. 100 °C,
Time 252000 sec
343.1 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 361.2 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
361.2 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 368.9 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
368.9 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 383.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
383.2 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 421.1 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
421.1 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 546.1 %
@Treatment Temp. 125 °C,
Time 252000 sec
546.1 %
@Treatment Temp. 257 °F,
Time 70.0 hour
ASTM Oil #1
 661.2 %
@Treatment Temp. 150 °C,
Time 252000 sec
661.2 %
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
100% Modulus 3.77 MPa547 psi
Tear Strength 43.6 kN/m249 pliDie C
 55.2 kN/m315 pliDie B
Compression Set  8.1 %
@Treatment Temp. 100 °C,
Time 79200 sec
8.1 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Solid
 10.7 %
@Treatment Temp. 125 °C,
Time 79200 sec
10.7 %
@Treatment Temp. 257 °F,
Time 22.0 hour
Solid
 12.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
12.2 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Solid
 22.2 %
@Treatment Temp. 100 °C,
Time 79200 sec
22.2 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Plied
 23 %
@Treatment Temp. 125 °C,
Time 79200 sec
23 %
@Treatment Temp. 257 °F,
Time 22.0 hour
Plied
 23.5 %
@Treatment Temp. 100 °C,
Time 252000 sec
23.5 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -27.2 °C-17.0 °F
Shrinkage  -9.30 %
@Treatment Temp. 150 °C,
Time 252000 sec
-9.30 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 -7.30 %
@Treatment Temp. 100 °C,
Time 252000 sec
-7.30 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 -6.60 %
@Treatment Temp. 125 °C,
Time 252000 sec
-6.60 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 -0.600 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
-0.600 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel A
 -0.400 %
@Treatment Temp. 100 °C,
Time 252000 sec
-0.400 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 0.90 %
@Treatment Temp. 125 °C,
Time 252000 sec
0.90 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 1.2 %
@Treatment Temp. 150 °C,
Time 252000 sec
1.2 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 7.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
7.7 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 15.9 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
15.9 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel B
 26.6 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
26.6 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL015 / 318225

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.