MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese IBC1000 kg-50000928 80% Sucrose Acetate Isobutyrate (SAIB) Solution in Ethyl Acetate
Categories: Fluid

Material Notes: CAS Number: 126-13-6

SAIB is a high purity carbohydrate. This sugar derivative, produced by esterification of natural sugar with Acetic and Isobutyric Anhydrides, is a mixture of different isomers with an approximate composition of sucrose diacetate hexaisobutyrate. SAIB 80% is a 80%solution of SAIB with 20% Ethyl Acetate (Ethyl Acetate purity min. 99.7%).

SAIB can be used for a wide range of applications. Major areas are inks, coatings and paper production. Common literature describes also the use in beverages and controlled-release formulations for pharmaceuticals. SAIB is employed as a modifier-extender leading to higher solids extending the film-forming polymer. The hardness of cellulose-nitrate films can be increased by the addition of SAIB. Flow properties are often improved and surface imperfections can be reduced. At more relevant temperatures the sucrose ester may serve as a plasticizer e.g. in printing inks for food packaging foils to improve adhesion and heat stability. SAIB´s advantageous features for coatings and inks may be: Low volatility of pure SAIB, resulting in higher solids content, Low color, Compatibility with most polymers and resins, oils and waxes. SAIB can also be added to hot-melt adhesives and coatings which are used to package items such as table flatware, tolls, machine parts, etc. The sucrose ester may lower the coating temperature and appears to have a stabilizing influence on the total hot-melt coatings. In such applications it may exhibit good color retention and stability on heat aging. SAIB can help efficiently to disperse pigments. The ester can support the formation of stable suspensions with good compatibility with binder resins in coating materials and inks. For the production of papers it serves as a clarifier and transparentizing agent due to a similar refractive index to cellulose fibers. It may increase the stability of the paper to heat and light as well as transparency and printability of the paper. The paper is usually impregnated or coated with a solution of SAIB in a low boiling solvent, such as an alcohol.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 - 1.09 g/ccDIN 51 757
Viscosity 16 - 23 cP
@Temperature 20.0 °C
Molecular Weight 846 g/mol
Vapor Pressure 0.0580 bar
@Temperature 20.0 °C
 0.201 bar
@Temperature 50.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point 104 °C
@Pressure 0.101 MPa
Flash Point 3.50 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.44
@Temperature 20.0 °C
nD; DIN 51 423, part 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese EBL 200 kg-50000931 80% Sucrose Acetate Isobutyrate (SAIB) Solution in Ethyl Acetate
American Maple, Rock (Sugar Maple)
Sugar Pine

WCELAN954 / 178025

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.