MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type H12 Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: Oversized Charpy specimens austenitized at 1010°C for 1 hr., air-cooled, and double tempered to indicated hardness in Charpy Impact notes prior to grinding to finished size

Key Words: UNS T20812, ASTM A681, FED QQ-T-570, SAE J437, SAE J438, SAE J467, DIN 1.2606, UNI X 35 CrMoW 05 KU, JIS SKD 62, B.S. BH 12 (UK)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.81 g/cc
 
Mechanical PropertiesOriginal ValueComments
Bulk Modulus 160 GPaTypical for steel.
Shear Modulus 80.0 GPaTypical for steel.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.30 - 0.40 %
Chromium, Cr 4.75 - 5.5 %
Iron, Fe 90.2 - 92.7 %As Balance
Molybdenum, Mo 1.25 - 1.75 %
Tungsten, W 1.0 - 1.7 %
Vanadium, V <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type H13 Hot Work Tool Steel
AISI Type H21 Tool Steel
AISI Type A2 Tool Steel
AISI Type H11 Hot Work Tool Steel, air or oil quenched from 995-1025°C
AISI Type H10 Chromium Hot Work Tool Steel (UNS T20810)

MSTH12A / 14075

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.