MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type H11 Hot Work Tool Steel, air or oil quenched from 995-1025°C
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: High hardenability, excellent toughness

Key Words: UNS T20811
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 642642Converted from Rockwell C hardness.
Hardness, Rockwell C 5656
Hardness, Vickers 621621
Tensile Strength, Ultimate 1990 MPa289000 psi
Tensile Strength, Yield 1650 MPa239000 psi
Elongation at Break 9.0 %9.0 %in 50 mm
Modulus of Elasticity 210 GPa30500 ksi
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.300.30Calculated
Machinability 45 - 55 %45 - 55 %Based on 1% carbon steel. as 100% machinability
Shear Modulus 81.0 GPa11700 ksiEstimated from elastic modulus
Charpy Impact 18.0 J13.3 ft-lbV-notch
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 25.0 - 95.0 °C
6.11 µin/in-°F
@Temperature 77.0 - 203 °F
 12.4 µm/m-°C
@Temperature 25.0 - 540 °C
6.89 µin/in-°F
@Temperature 77.0 - 1000 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  24.6 W/m-K
@Temperature 215 °C
171 BTU-in/hr-ft²-°F
@Temperature 419 °F
 42.0 W/m-K
@Temperature 23.0 °C
291 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 540 - 650 °C1000 - 1200 °FTempering Temperature
 995 - 1025 °C1820 - 1877 °FHardening Temperature
Annealing Temperature 845 - 900 °C1550 - 1650 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.33 - 0.43 %0.33 - 0.43 %
Chromium, Cr 5.2 %5.2 %
Iron, Fe 93 %93 %As Balance
Molybdenum, Mo 1.35 %1.35 %
Vanadium, V 0.45 %0.45 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type H13 Hot Work Tool Steel
AISI Type A2 Tool Steel
AISI Type H12 Hot Work Tool Steel
Latrobe LSS™ H11 Hot Work Tool Steel (ASTM H11)
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C

MSTH11A / 14074

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.