MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips Sumika Marlex® HLN-200 Polypropylene Random Copolymer, Antistatic  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Polypropylene Homopolymer, Antistatic, Nucleated, Controlled Rheology

Applications: Formulated for closures, food containers, housewares, and toys

Comments: Meets FDA Regulation 21 CFR 177.1520 and is suitable for food packaging applications at temperatures not exceeding 212°F (100°C), Listed in the Drug Master File, UL listed, 1.5 mm thick, natural, RTI 65°C, Flame Rating 94 HB

The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Data provided by Phillips Sumika Polypropylene Company (PSPC).

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.907 g/cc
@Thickness 3.17 mm
0.0328 lb/in³
@Thickness 0.125 in
injection molded specimen; ASTM D1505
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.0 MPa
@Thickness 3.17 mm
5370 psi
@Thickness 0.125 in
Type 1 Specimen, Rate: 2"/min; injection-molded specimen; ASTM D638
Flexural Modulus 1.999 GPa
@Thickness 3.17 mm
289.9 ksi
@Thickness 0.125 in
Tangent; Rate 0.5"/min; injection-molded specimen; ASTM D790
Izod Impact, Notched 0.270 J/cm
@Thickness 3.17 mm
0.506 ft-lb/in
@Thickness 0.125 in
injection molded specimen; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL RTI, natural color
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
@Thickness 3.17 mm
250 °F
@Thickness 0.125 in
injection molded specimen; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
natural color
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips Sumika Marlex® JM97A Polypropylene Random Copolymer, UV Stabilized
Braskem RP350 Polypropylene Random Copolymer
Dow DS6D82 Polypropylene Random Copolymer Resin
Dow R792-35RNA Polypropylene Random Copolymer Resin
Epsilon Polymers RN-355 Polypropylene Random Copolymer

PCHEVS56 / 20385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.