MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Universal Wire Works 5Al-2.5Sn (AMS 4953) Titanium Alloy Filler Metal
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Universal Ti 5Al-2.5Sn titanium alloy is easily joined with the gas tungsten arc, gas metal arc or resistance welding processes. 100% joint efficiency can be obtained provided proper shielding procedures are used. Alloy 4953 is often employed for applications where weldability and oxidation resistance is of major interest. Good high temperature strength and stability are trademarks of this alloy.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 827 MPa120000 psiAnnealed
Tensile Strength, Yield 793 MPa
@Strain 0.2 %
115000 psi
@Strain 0.2 %
Annealed
Elongation at Break 10 %10 %Annealed
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 5.75 %<= 5.75 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.50 %<= 0.50 %
Nitrogen, N <= 0.050 %<= 0.050 %
Oxygen, O <= 0.175 %<= 0.175 %
Tin, Sn <= 3.0 %<= 3.0 %
Titanium, Ti >= 90.43 %>= 90.43 %As Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Universal Wire Works Commercially Pure (AMS 4951) Titanium Alloy Filler Metal
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed
304 Stainless Steel (UNS S30400); Annealed Wire

NUWW256 / 19714

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.