MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Journal Bearing Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Journal Bearing Oil is a high quality, high viscosity index, paraffinic-based lubricant. It incorporates highly effective deposit control antioxidants and rust inhibitors as well as a pour point depressant and viscosity index improver for outstanding year round railroad journal box lubrication.

This product is formulated to exceed the requirements of Association of American Railroads (AAR) Specification M 963 84 for All-Year Journal Box Lubricating Oil.

Chevron Journal Bearing Oil is designed for use in the journal boxes of railcars using plain bearings, not antifriction bearings. The journal box is filled with a waste material which is saturated with Chevron Journal Bearing Oil. The waste, which is against the journal, is heated by friction as the car rolls, causing the oil to slowly feed into the journal bearing. For this reason, a high viscosity index oil is critical. It must have good fluidity at low temperatures and not think excessively at high temperatures.

Chevron Journal Bearing Oil passes:

  • ASTM D 665 Rust Test
  • ASTM D 1748 Corrosion Humidity Cabinet Test

Applications

Chevron Journal Bearing Oil is recommended for the lubrication of journal bearings on the trucks of railcars where a lubricant meeting the requirements of AAR Specification M-963-84 for All-Year Journal box lubricating oil is recommended.

Key Words: CPS Number: 233803; MSDS Number: 4626
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31 °
Viscosity Measurement 117Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 320 SUS
Saybolt Viscosity at 210°F 56 SUS
Kinematic Viscosity at 40°C (104°F) 60.91 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 8.72 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -39.0 °CASTM D97
Flash Point 237 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 AAR 963 Oil ISO Grade 46
ChevronTexaco Journaltex® HD 57

WCHEV090 / 74705

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.