MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP)  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique properties of this material are due primarily to the inherent rigid-rod structure. PrimoSpire® SRP is differentiated from other thermoplastics by outstanding mechanical properties without fiber reinforcement, scratch resistance, excellent solvent resistance and exceptional low temperature performance. In addition, PrimoSpire® SRP has great thermal stability, is non-combustible, has higher specific strength than many of the common structural materials and machines easily.

Features: Ductile; Flame Retardant; Good Chemical Resistance; High Stiffness; High Strength; Scratch Resistant

Uses: Aircraft Applications; Connectors; Electrical/Electronic Applications; Film; Gears; Housings; Medical/Healthcare Applications; Semiconductor Molding Compounds

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ISO 62
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 152 MPa22000 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Tensile Modulus 5.52 GPa801 ksiASTM D638
Flexural Strength 234 MPa33900 psiASTM D790
Flexural Modulus 6.00 GPa870 ksiASTM D790
Izod Impact, Notched 0.590 J/cm1.11 ft-lb/inASTM D256
Izod Impact, Unnotched 16.0 J/cm30.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 7.00e+15 ohm-cm>= 7.00e+15 ohm-cmASTM D257
Dielectric Constant  3.01
@Frequency 1e+6 Hz
3.01
@Frequency 1e+6 Hz
ASTM D150
 3.11
@Frequency 1000 Hz
3.11
@Frequency 1000 Hz
ASTM D150
 3.12
@Frequency 60 Hz
3.12
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm508 kV/inASTM D149
Dissipation Factor  0.0070
@Frequency 60 Hz
0.0070
@Frequency 60 Hz
ASTM D150
 0.0070
@Frequency 1000 Hz
0.0070
@Frequency 1000 Hz
ASTM D150
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C17.2 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 151 °C304 °FUnannealed; ASTM D648
Glass Transition Temp, Tg 168 °C334 °FASTM E1356
Oxygen Index 55 %55 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 310 °C590 °F
Middle Barrel Temperature 324 °C615 °F
Front Barrel Temperature 335 °C635 °F
Nozzle Temperature 341 °C646 °F
Melt Temperature 343 - 349 °C649 - 660 °F
Mold Temperature 129 - 146 °C264 - 295 °F
Drying Temperature 149 °C
@Time 10800 sec
300 °F
@Time 3.00 hour
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural
FormPellets; Powder
Injection RateSlow-Moderate
Processing TechniqueCompression Molding; Film Extrusion; Injection Molding
 Machining; Profile Extrusion; Wire & Cable Extrusion
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA A950 LCP, Unfilled
Syensqo (Solvay Specialty Polymers) Torlon® 4203 Polyamide-imide (PAI)
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP)
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-120 Self-Reinforced Polyphenylene
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-9250 Polyphenylene, Self-Reinforced (SRP)

PSOL8Y7230 / 176961

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.