MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta MC514MG Phenolic Glass Laminate Sheet
Categories: Polymer; Thermoset; Phenolic

Material Notes: MC514MG is a glass phenolic, semi-conductive laminate which was designed for corona discharge in the power generation industry. The graphitic carbon additive in the resin system enables easy installation in the slots and provides the necessary conductivity to safely remove harmful charges from the system.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Phenolic, Micarta, Graphite Carbon
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
@Thickness 12.7 mm
ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 110
@Thickness 6.35 mm
ASTM D785
Flexural Strength 25000 psi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 34000 psi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Compressive Strength 48000 psi
@Thickness 12.7 mm
Flatwise; ASTM D695 Condition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Mechanical with Impact 155 °CUL Bulletin 746b
 
Descriptive Properties
Bonding Strength1100[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta BR60 Phenolic Canvas Laminate Sheet
Norplex-Micarta MC511AF Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC507U Silicone Glass Laminate Sheet, NEMA G-7
Norplex-Micarta MC330 Phenolic Cotton Laminate Sheet

PNORPM060 / 192817

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.