MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta MC330 Phenolic Cotton Laminate Sheet
Categories: Polymer; Thermoset; Phenolic

Material Notes: Grade MC330 is a cotton cloth/phenolic resin composite which is specially processed to be used in cryogenic applications. Such applications include spacers for installation of liquid oxygen apparatus where temperatures are as low as minus 320F.

Information provided by Norplex-Micarta

Key Words: Cotton, Phenolic, Micarta, Cryogenic
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc
@Thickness 12.7 mm
1.37 g/cc
@Thickness 0.500 in
ASTM D792
Moisture Absorption 3.50 %
@Thickness 1.57 mm
3.50 %
@Thickness 0.0620 in
ASTM D570 Condition D1-24/23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100
@Thickness 6.35 mm
100
@Thickness 0.250 in
ASTM D785
Tensile Strength  66.9 MPa
@Thickness 3.17 mm
9700 psi
@Thickness 0.125 in
CrossWise; ASTM D638 Condition A
 82.7 MPa
@Thickness 3.17 mm
12000 psi
@Thickness 0.125 in
LengthWise; ASTM D638 Condition A
Flexural Strength  117 MPa
@Thickness 1.57 mm
17000 psi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 124 MPa
@Thickness 1.57 mm
18000 psi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Flexural Modulus  10.3 GPa
@Thickness 1.57 mm
1500 ksi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 11.0 GPa
@Thickness 1.57 mm
1600 ksi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Compressive Strength 234 MPa
@Thickness 12.7 mm
34000 psi
@Thickness 0.500 in
Flatwise; ASTM D695 Condition A
Shear Strength 96.5 MPa
@Thickness 1.57 mm
14000 psi
@Thickness 0.0620 in
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched  0.934 J/cm
@Thickness 12.7 mm
1.75 ft-lb/in
@Thickness 0.500 in
CrossWise; ASTM D256 Condition E-48/50
 1.04 J/cm
@Thickness 12.7 mm
1.95 ft-lb/in
@Thickness 0.500 in
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  5.91 kV/mm
@Thickness 1.57 mm
150 kV/in
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
 15.7 kV/mm
@Thickness 1.57 mm
400 kV/in
@Thickness 0.0620 in
ASTM D149 Condition A
Dielectric Breakdown  5000 V
@Thickness 1.57 mm
5000 V
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
 20000 V
@Thickness 1.57 mm
20000 V
@Thickness 0.0620 in
ASTM D149 Condition A
Comparative Tracking Index 155 V
@Thickness 3.17 mm
155 V
@Thickness 0.125 in
ASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Thickness 3.17 mm
11.1 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 22.0 µm/m-°C
@Thickness 3.17 mm
12.2 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
UL RTI, Mechanical with Impact 125 °C257 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
 
Descriptive Properties
Bonding Strength2300[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1340 Steel, normalized at 870°C (1600°F), air cooled, 25 mm (1 in.) round
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Norplex-Micarta BR60 Phenolic Canvas Laminate Sheet
Norplex-Micarta MC223 Phenolic Cotton Laminate Sheet

PNORPM024 / 192781

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.