MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Esenttia 01H41 Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Characteristics: Low melt flow rate Homopolymer polypropylene with excellent mechanical properties and color, excellent gage control and high melt strength.

Recommended for: Extrusion of strapping, sheets, Cartonplast, extrusion thermoforming, extrusion blow molding of bottles, injection molding of heels, extrusion and injection molding general purpose applications.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 1.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238B
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 33.78 MPa50 mm/min; ASTM D638
Elongation at Yield 10.5 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1447.9 MPa1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 48.04 J/mASTM D256-A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H05H-01 Polypropylene Homopolymer
Esenttia 03H82 Homopolymer Polypropylene
Braskem F008F Homopolymer Polypropylene
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4017 Polypropylene

PESEN001 / 184573

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.