MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Bapolene PP4062 is a high flow general purpose injection molding homopolyper polypropylene. This product meets US FDA 21 CFR 177.1520.

Applications: Consumer Applications; Household Goods; Rigid Packaging.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Antistatic; Fast Molding Cycle; Food Contact Acceptable; General Purpose; Homopolymer; Nucleated
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D-1505
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.5 MPa5000 psiASTM D-638
Flexural Modulus 1.52 GPa220 ksiASTM D-790
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/in@73°F; ASTM D-256
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned
Borealis RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Bamberger Polymers Bapolene® 4072 Polypropylene, Injection Grade

PBP3B210 / 20813

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.