MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 99 Mildly Activated Rosin Flux, Type RMA
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • A mildly activated rosin flux for general-purpose soldering of PCB's, wire, cable, and semiconductors, and hand soldering applications.
  • Excellent for a variety of metals including copper, gold, nickel alloys, silver, and tin.
  • Can be used for automated and manual soldering operations.
  • Flux conforms to IPC-ANSI-J-STD-004, Type ROL1.
Description: Superior No. 99 RMA Flux consists of a homogeneous solution of water-white rosin in a multi-component solvent system with a brominated organic activator. It is completely chloride-free. The flux is widely used in electronic applications requiring excellent soldering activity and yielding residues with high water-extract resistivities. Superior No. 99 RMA Flux becomes active above 175°C/340°F, attaining peak activity in the temperature range 200-260°C/390-500°F, where it promotes excellent solderability. It can also be used for high-temperature soldering applications, such as mag-wire tinning at temperatures in the 400-430°C/750-800°F range.

Applications: Superior No. 99 RMA Flux is an excellent choice for soldering printed circuit boards (PCBs), wire leads, cables, and component tinning. Superior No. 99 RMA Flux can be used to solder many different metals and alloys including copper, gold, alloy 42, alloy 51, nickel alloys, and other metals commonly used in electronics applications.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 - 0.920 g/cc0.880 - 0.920 g/cc
Density 0.899 g/cc0.0325 lb/in³
Solids Content 43.5 - 47.5 %43.5 - 47.5 %
 
Thermal PropertiesMetricEnglishComments
Boiling Point 82.3 °C180 °F
Flash Point 12.0 °C53.6 °FTCC Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 260 °C392 - 500 °FSoldering Range
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
FormLight Brown Liquid
ResiduesNon-Corrosive, Non-Conductive
Spread Factor>90
Water Extract Resistivity150000 ohm/cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX040 / 185724

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.