Physical Properties | Metric | English | Comments |
---|
Density | 1.054 g/cc @Temperature 120 °C | 0.03808 lb/in³ @Temperature 248 °F |
| 1.067 g/cc @Temperature 110 °C | 0.03855 lb/in³ @Temperature 230 °F |
| 1.08 g/cc @Temperature 100 °C | 0.0390 lb/in³ @Temperature 212 °F |
| 1.093 g/cc @Temperature 90.0 °C | 0.03949 lb/in³ @Temperature 194 °F |
| 1.106 g/cc @Temperature 80.0 °C | 0.03996 lb/in³ @Temperature 176 °F |
| 1.119 g/cc @Temperature 70.0 °C | 0.04043 lb/in³ @Temperature 158 °F |
| 1.131 g/cc @Temperature 60.0 °C | 0.04086 lb/in³ @Temperature 140 °F |
| 1.144 g/cc @Temperature 50.0 °C | 0.04133 lb/in³ @Temperature 122 °F |
| 1.156 g/cc @Temperature 40.0 °C | 0.04176 lb/in³ @Temperature 104 °F |
| 1.162 g/cc @Temperature 35.0 °C | 0.04198 lb/in³ @Temperature 95.0 °F |
| 1.168 g/cc @Temperature 30.0 °C | 0.04220 lb/in³ @Temperature 86.0 °F |
| 1.174 g/cc @Temperature 25.0 °C | 0.04241 lb/in³ @Temperature 77.0 °F |
| 1.181 g/cc @Temperature 20.0 °C | 0.04267 lb/in³ @Temperature 68.0 °F |
| 1.187 g/cc @Temperature 15.0 °C | 0.04288 lb/in³ @Temperature 59.0 °F |
| 1.199 g/cc @Temperature 5.00 °C | 0.04332 lb/in³ @Temperature 41.0 °F |
| 1.206 g/cc @Temperature 0.000 °C | 0.04357 lb/in³ @Temperature 32.0 °F |
| 1.93 g/cc @Temperature 10.0 °C | 0.0697 lb/in³ @Temperature 50.0 °F |
Solubility in Water | 1.5 % | 1.5 % |
| 6.5 % | 6.5 % |
Viscosity | 0.42 cP @Temperature 120 °C | 0.42 cP @Temperature 248 °F |
| 0.44 cP @Temperature 110 °C | 0.44 cP @Temperature 230 °F |
| 0.48 cP @Temperature 100 °C | 0.48 cP @Temperature 212 °F |
| 0.52 cP @Temperature 90.0 °C | 0.52 cP @Temperature 194 °F |
| 0.57 cP @Temperature 80.0 °C | 0.57 cP @Temperature 176 °F |
| 0.62 cP @Temperature 70.0 °C | 0.62 cP @Temperature 158 °F |
| 0.69 cP @Temperature 60.0 °C | 0.69 cP @Temperature 140 °F |
| 0.76 cP @Temperature 50.0 °C | 0.76 cP @Temperature 122 °F |
| 0.84 cP @Temperature 40.0 °C | 0.84 cP @Temperature 104 °F |
| 0.90 cP @Temperature 35.0 °C | 0.90 cP @Temperature 95.0 °F |
| 0.96 cP @Temperature 30.0 °C | 0.96 cP @Temperature 86.0 °F |
| 1.03 cP @Temperature 25.0 °C | 1.03 cP @Temperature 77.0 °F |
| 1.12 cP @Temperature 20.0 °C | 1.12 cP @Temperature 68.0 °F |
| 1.21 cP @Temperature 15.0 °C | 1.21 cP @Temperature 59.0 °F |
| 1.31 cP @Temperature 10.0 °C | 1.31 cP @Temperature 50.0 °F |
| 1.43 cP @Temperature 5.00 °C | 1.43 cP @Temperature 41.0 °F |
| 1.55 cP @Temperature 0.000 °C | 1.55 cP @Temperature 32.0 °F |
Molecular Weight | 92.53 g/mol | 92.53 g/mol |
Vapor Pressure | 0.00456 bar @Temperature 0.000 °C | 3.42 torr @Temperature 32.0 °F |
| 0.00648 bar @Temperature 5.00 °C | 4.86 torr @Temperature 41.0 °F |
| 0.00882 bar @Temperature 10.0 °C | 6.61 torr @Temperature 50.0 °F |
| 0.0122 bar @Temperature 15.0 °C | 9.12 torr @Temperature 59.0 °F |
| 0.0165 bar @Temperature 20.0 °C | 12.4 torr @Temperature 68.0 °F |
| 0.0220 bar @Temperature 25.0 °C | 16.5 torr @Temperature 77.0 °F |
| 0.0290 bar @Temperature 30.0 °C | 21.7 torr @Temperature 86.0 °F |
| 0.0379 bar @Temperature 35.0 °C | 28.4 torr @Temperature 95.0 °F |
| 0.0491 bar @Temperature 40.0 °C | 36.9 torr @Temperature 104 °F |
| 0.0798 bar @Temperature 50.0 °C | 59.9 torr @Temperature 122 °F |
| 0.126 bar @Temperature 60.0 °C | 94.2 torr @Temperature 140 °F |
| 0.192 bar @Temperature 70.0 °C | 144 torr @Temperature 158 °F |
| 0.285 bar @Temperature 80.0 °C | 214 torr @Temperature 176 °F |
| 0.412 bar @Temperature 90.0 °C | 309 torr @Temperature 194 °F |
| 0.583 bar @Temperature 100 °C | 437 torr @Temperature 212 °F |
| 0.807 bar @Temperature 110 °C | 605 torr @Temperature 230 °F |
| 1.09 bar @Temperature 120 °C | 821 torr @Temperature 248 °F |
Surface Tension | 0.035 dynes/cm | 0.035 dynes/cm |
|
Chemical Properties | Metric | English | Comments |
---|
Critical Pressure | 49.0 bar | 36800 torr |
Critical Temperature | 327 °C | 621 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 2.90e+7 ohm-cm | 2.90e+7 ohm-cm |
Dielectric Constant | 20.8 @Temperature 21.5 °C | 20.8 @Temperature 70.7 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Heat of Vaporization | 420 J/g @Temperature 120 °C | 181 BTU/lb @Temperature 248 °F |
| 427 J/g @Temperature 110 °C | 184 BTU/lb @Temperature 230 °F |
| 435 J/g @Temperature 100 °C | 187 BTU/lb @Temperature 212 °F |
| 442 J/g @Temperature 90.0 °C | 190 BTU/lb @Temperature 194 °F |
| 449 J/g @Temperature 80.0 °C | 193 BTU/lb @Temperature 176 °F |
| 456 J/g @Temperature 70.0 °C | 196 BTU/lb @Temperature 158 °F |
| 462 J/g @Temperature 60.0 °C | 199 BTU/lb @Temperature 140 °F |
| 469 J/g @Temperature 50.0 °C | 202 BTU/lb @Temperature 122 °F |
| 475 J/g @Temperature 40.0 °C | 204 BTU/lb @Temperature 104 °F |
| 478 J/g @Temperature 35.0 °C | 206 BTU/lb @Temperature 95.0 °F |
| 484 J/g @Temperature 25.0 °C | 208 BTU/lb @Temperature 77.0 °F |
| 487 J/g @Temperature 20.0 °C | 210 BTU/lb @Temperature 68.0 °F |
| 487 J/g @Temperature 30.0 °C | 210 BTU/lb @Temperature 86.0 °F |
| 491 J/g @Temperature 15.0 °C | 211 BTU/lb @Temperature 59.0 °F |
| 494 J/g @Temperature 10.0 °C | 213 BTU/lb @Temperature 50.0 °F |
| 497 J/g @Temperature 5.00 °C | 214 BTU/lb @Temperature 41.0 °F |
| 500 J/g @Temperature 0.000 °C | 215 BTU/lb @Temperature 32.0 °F |
Specific Heat Capacity | 1.19 J/g-°C @Temperature 100 °C | 0.284 BTU/lb-°F @Temperature 212 °F |
| 1.47 J/g-°C @Temperature 0.000 °C | 0.351 BTU/lb-°F @Temperature 32.0 °F |
| 1.48 J/g-°C @Temperature 5.00 °C | 0.354 BTU/lb-°F @Temperature 41.0 °F |
| 1.50 J/g-°C @Temperature 10.0 °C | 0.359 BTU/lb-°F @Temperature 50.0 °F |
| 1.51 J/g-°C @Temperature 15.0 °C | 0.361 BTU/lb-°F @Temperature 59.0 °F |
| 1.53 J/g-°C @Temperature 20.0 °C | 0.366 BTU/lb-°F @Temperature 68.0 °F |
| 1.54 J/g-°C @Temperature 25.0 °C | 0.368 BTU/lb-°F @Temperature 77.0 °F |
| 1.56 J/g-°C @Temperature 30.0 °C | 0.373 BTU/lb-°F @Temperature 86.0 °F |
| 1.58 J/g-°C @Temperature 35.0 °C | 0.378 BTU/lb-°F @Temperature 95.0 °F |
| 1.60 J/g-°C @Temperature 40.0 °C | 0.382 BTU/lb-°F @Temperature 104 °F |
| 1.64 J/g-°C @Temperature 50.0 °C | 0.392 BTU/lb-°F @Temperature 122 °F |
| 1.68 J/g-°C @Temperature 60.0 °C | 0.402 BTU/lb-°F @Temperature 140 °F |
| 1.72 J/g-°C @Temperature 70.0 °C | 0.411 BTU/lb-°F @Temperature 158 °F |
| 1.77 J/g-°C @Temperature 80.0 °C | 0.423 BTU/lb-°F @Temperature 176 °F |
| 1.82 J/g-°C @Temperature 90.0 °C | 0.435 BTU/lb-°F @Temperature 194 °F |
| 1.87 J/g-°C @Temperature 100 °C | 0.447 BTU/lb-°F @Temperature 212 °F |
| 1.92 J/g-°C @Temperature 110 °C | 0.459 BTU/lb-°F @Temperature 230 °F |
| 1.97 J/g-°C @Temperature 120 °C | 0.471 BTU/lb-°F @Temperature 248 °F |
Melting Point | -57.0 °C | -70.6 °F |
Boiling Point | 88.0 °C | 190 °F |
| 116 °C @Pressure 1.013 MPa | 241 °F @Pressure 146.9 psi |
Decomposition Temperature | >= 225 °C | >= 437 °F |
Flash Point | 31.0 °C | 87.8 °F |
Ignition Temperature | >= 385 °C | >= 725 °F |
|
Descriptive Properties |
---|
Appearance | Clear liquid, free from visible matter or particles |
Coefficient of volume expansion | 0.00094 |
Color | <15 |
Combustion heat | 19 kJ/g |
Composition | <100 mg/kg |
| >99.8% |
Flammability limits | 3.8-21% |
Latent heat of evaporation | .42 kJ/g |
Partition coefficient P | 0.3 Log P o/w |