MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3D Systems NextDent SG (Surgical Guide) Dental Material
Categories: Other Engineering Material

Material Notes: NextDent SG is a biocompatible Class I material, developed for the printing of Surgical Guides for implant surgery use. Because of the high precision of this material it is easy to insert drill sleeves, directly after printing. Enabling even greater precision during surgery. The properties of NextDent SG will not change by using disinfectants. In addition, the material can also be sterilized using standard autoclave protocols. The use of an autoclave does not affect the dimensional stability, therefore NextDent SG can be used in every operating theatre. Available in color Translucent Orange.

Information provided by 3D Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength >= 50.0 MPa>= 7250 psiRequirement, Ultimate; ISO 20795-1
 85.0 MPa12300 psiResult, Ultimate; ISO 20795-1
Flexural Modulus >= 1.50 GPa>= 218 ksiRequirement; ISO 20795-1
 2.118 GPa307.2 ksiResult; ISO 20795-1
 
Descriptive Properties
Residual monomer< 0.1 %Result, ISO 20795-1
 = 2.2 %Requirement, ISO 20795-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAPPR3210 / 239178

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.