NextDent SG is a biocompatible Class I material, developed for the printing of Surgical Guides for implant surgery use. Because of the high precision of this material it is easy to insert drill sleeves, directly after printing. Enabling even greater precision during surgery. The properties of NextDent SG will not change by using disinfectants. In addition, the material can also be sterilized using standard autoclave protocols. The use of an autoclave does not affect the dimensional stability, therefore NextDent SG can be used in every operating theatre. Available in color Translucent Orange.Information provided by 3D Systems |