MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes:
  • injection molding grade
  • 20 % Glass fiber reinforced
  • good heat resistance
  • low coefficent of linear thermal expansion
Application
  • Automotive engineering
  • Injection molded engineering parts

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 993s; ISO 868
Hardness, Shore D 7015s; ISO 868
Tensile Strength at Break 64.0 MPaISO 527-1/-2
Tensile Strength, Yield 64.0 MPaparallel; ISO 527-3
Elongation at Break 25 %ISO 527-1/-2
Charpy Impact Unnotched 15.0 J/cm²ISO 179/1eU
 8.20 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.70 J/cm²ISO 179/1eA
 1.40 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°CISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Drying Temperature 70.0 - 110 °C
Dry Time 1.00 - 2.00 hourDry Air Dryer
Moisture Content <= 0.050 %
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 India
 Near East/Africa
 South and Central America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 481 Polyurethane
Arkema Pebax® 2533 SA 01 MED Polyether Block Amide (PEBA)
Covestro Desmopan® 192 Thermoplastic Polyurethane
Covestro Desmopan® 5377A Polyurethane
Covestro Desmopan® 9386A Polyurethane

PB09796 / 92636

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.