MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro Desmopan® 5377A Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; improved microbial resistance; Improved hydrolysis resistance; Application; Textile coating; Wristwatch straps; hard - soft systems

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777ISO 868
Hardness, Shore D 2828ISO 868
Tensile Strength, Ultimate 27.0 MPa3920 psi200 mm/min; DIN 53504
Tensile Stress at Strain  1.30 MPa
@Strain 10 %
189 psi
@Strain 10 %
200 mm/min; DIN 53504
 3.60 MPa
@Strain 50 %
522 psi
@Strain 50 %
200 mm/min; DIN 53504
 4.90 MPa
@Strain 100 %
711 psi
@Strain 100 %
200 mm/min; DIN 53504
 8.90 MPa
@Strain 300 %
1290 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 644 %644 %200 mm/min; DIN 53504
Tensile Modulus  0.0210 GPa
@Temperature 60.0 °C
3.05 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.0290 GPa
@Temperature 20.0 °C
4.21 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.180 GPa
@Temperature -20.0 °C
26.1 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Rebound 45 %45 %Resilience; ISO 4662
Tear Strength 40.0 kN/m228 pli500 mm/min; ISO 34-1
Abrasion 8080mm³, Method A; ISO 4649
Compression Set  20 %
@Temperature 23.0 °C
20 %
@Temperature 73.4 °F
72 hr; ISO 815
 29 %
@Temperature 70.0 °C
29 %
@Temperature 158 °F
24 hr, Method C; ISO 815
 43 %
@Temperature 70.0 °C
43 %
@Temperature 158 °F
24 hr; ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 190 °C338 - 374 °FExtrusion
 180 - 200 °C356 - 392 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer
BASF Petra® 130 30% Glass Filled PET
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)

PB09765 / 92605

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.