MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Materion Brushform® 290 Beryllium Copper Alloy Strip; TM02 Temper (UNS C17200)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: Mill Hardened
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%
Stress Relaxation after 1000 hrs @ 200°C: 76%
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 0
Formability Ratio (bad Way): 0
Superficial Hardness: 30N 46-54

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-194
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 25 - 3425 - 34
Hardness, Vickers 255 - 339255 - 339
Tensile Strength, Ultimate >= 820 MPa>= 119000 psi
Tensile Strength, Yield 650 - 800 MPa94300 - 116000 psi
Elongation at Break 14 - 30 %14 - 30 %
Modulus of Elasticity 131 GPa19000 ksi
Fatigue Strength 290 - 330 MPa
@# of Cycles 1.00e+8
42100 - 47900 psi
@# of Cycles 1.00e+8
Reverse Bending (R=1)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 - 0.0000101 ohm-cm0.00000660 - 0.0000101 ohm-cm17-26% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C1600 - 1800 °F
Solidus 870 °C1600 °F
Liquidus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.8 - 2.0 %1.8 - 2.0 %
Co + Ni >= 0.20 %>= 0.20 %
Co + Ni + Fe <= 0.60 %<= 0.60 %
Copper, Cu 98 %98 %as balance
Lead, Pb <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten, W
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200)
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM06 Temper (UNS C17200)
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM04 Temper (UNS C17200)
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200)

NBB638 / 15257

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.