Treatment required for max strength: Mill Hardened Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99% Stress Relaxation after 1000 hrs @ 200°C: 78% Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 3.5 Formability Ratio (bad Way): 3 Superficial Hardness: 30N 55-62Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman. Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |