MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Strator® A-3 XC N7 Polyamide 66 (Nylon 66), 30% Long Carbon Fiber, Heat Stabilizer  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Carbon Fiber Filled

Material Notes: Strator® A-3 XC N7, a long carbon fiber filled, heat stabilized high-flow PA, can easily be processed on most injection molding machines.

This material achieves extremely high mechanical and thermal properties, in combination with ease of processing and fast cycle times. It exhibits high strength, stiffness and impact strength at high temperatures; excellent creep and fatigue resistance; isotropic mechanical properties and reduced isotropic shrinkage; high shear strength and high burst pressure; and an excellent surface finish.

Creep Resistant; Electrically Insulating; Fatigue Resistant; High Impact Resistance; High Rigidity; High Stiffness; High Tensile Strength; Hot Water Moldability; Low CLTE; Low Warpage

Uses: Aircraft Applications; Automotive Applications; Automotive Instrument Panel; Gears

Processing: Injection Molding

Availability: Europe

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
 1.28 g/cc0.0462 lb/in³ISO 1183
Moisture Absorption 1.70 %1.70 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0025 cm/cm0.0025 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 300 MPa43500 psiISO 527-2
Elongation at Break 1.8 %1.8 %ISO 527-2
Tensile Modulus 24.0 GPa3480 ksiISO 527-2
Flexural Strength 400 MPa58000 psiISO 178
Flexural Modulus 22.5 GPa3260 ksiISO 178
Charpy Impact Unnotched 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 ohm100 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 300 °C518 - 572 °F
Middle Barrel Temperature 270 - 300 °C518 - 572 °F
Front Barrel Temperature 285 - 310 °C545 - 590 °F
Nozzle Temperature 285 - 320 °C545 - 608 °F
Melt Temperature <= 310 °C<= 590 °F
Mold Temperature 80.0 - 140 °C176 - 284 °F
Drying Temperature 110 °C
@Time 14400 sec
230 °F
@Time 4.00 hour
Moisture Content 0.10 %0.10 %
 
Descriptive Properties
FormsPellets
Suggested Max Regrind (%)15

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight

PSOL8Y6413 / 193334

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.