MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo CALIBRE™ 320 UV Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 302 UV polycarbonate resin contains a proprietary UV stabilization package that combines industry standard stabilization against ultraviolet radiation with low plate-out and discoloration during processing. This will result in less downtime for cleaning and easier processing. This product is designed for co-extrusion as a 50 µm thick layer on standard PC for use in solid and multi-wall sheets.

Main Characteristics:

  • Very low plate-out
  • Very high thermal stability
  • Very high color stability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 72.0 MPa10400 psiISO 527-2/50
Tensile Strength, Yield 70.0 MPa10200 psiISO 527-2/50
Elongation at Break 150 %150 %ISO 527-2/50
Elongation at Yield 6.0 %6.0 %ISO 527-2/50
Tensile Modulus 2.50 GPa363 ksiISO 527-2/1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FUnannealed; ISO 75-2/A
 128 °C262 °FAnnealed; ISO 75-2/A
Vicat Softening Point 139 °C282 °FISO 306/B50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PC-HT A 1000/500 High Heat Polycarbonate
Plastcom SLOVALEN PC 81 T 15 PP, 15% mineral filling
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate, High Heat
Overview of materials for Acrylic, General Purpose, Molded

PZZDWST043 / 142252

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.