MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALTECH® PC-HT A 1000/500 High Heat Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, High Heat

Material Notes: Base Polymer: High Heat Polycarbonate

Special Features: High heat stabilized

Market Segment: Automotive, Lighting

Typical Applications: Housings, Light switches

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Time 86400 sec
0.0040 - 0.0070 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 330 °C
17 g/10 min
@Load 4.76 lb,
Temperature 626 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 70.0 MPa10200 psiISO 527
Elongation at Yield 7.0 %7.0 %ISO 527
Tensile Modulus 2.50 GPa363 ksiISO 527
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 148 °C298 °FISO 75-1/-2
Vicat Softening Point 166 °C331 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 340 °C608 - 644 °FInjection molding
Mold Temperature 100 - 130 °C212 - 266 °FInjection molding
Drying Temperature  >= 120 °C
@Time 7200 - 10800 sec
>= 248 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 >= 130 °C
@Time 14400 - 43200 sec
>= 266 °F
@Time 4.00 - 12.0 hour
air circulating dryer
 
Descriptive Properties
Base PolymerHigh Heat Polycarbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 200-23 Polycarbonate Resin
Trinseo CALIBRE™ 200-6 Polycarbonate Resin
Trinseo CALIBRE™ 201-10 Polycarbonate Resin
Trinseo CALIBRE™ 201-22 Polycarbonate Resin
Trinseo CALIBRE™ 201-6 Polycarbonate Resin

PALBIS8827 / 242886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.