MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

PoolKemie POLIMOLD TR 70 Polyurethane rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Introduction: Two component room temperature vulcanizing poly-urethane rubber which cures with addition of the appropriate hardener. Once cured, this rubber becomes flexible and resistant, free from air bubbles and imperfections. It is suitable in the manufacture of moulds for production of articles made of plaster and cement thanks to its accurate reproduction of fine details and due to its extremely low linear shrinkage.

Application: POLIMOLD TR is specially suited for production of decorative plaster subjects, religious articles, statues, pottery, artistic ceramics, sanitary, precast concrete, garden ornaments, etc. Types characterized by high Shore A hardness value, are suited for reproduction of large-sized patterns.

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccmixture A+B
Viscosity 4000 cP4000 cPmixture A+B
Linear Mold Shrinkage <= 0.010 cm/cm<= 0.010 in/inafter 5 days ageing; ISO 4823
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 67 - 7367 - 73
Elongation at Break >= 250 %>= 250 %
Tear Strength 6.00 - 8.00 kN/m34.2 - 45.6 pliDIN 53515
 
Processing PropertiesMetricEnglishComments
Cure Time 420 - 600 min7.00 - 10.0 hourHardening time
 1440 min24.0 hourDemoulding time
Pot Life 20.0 min20.0 minmixture A+B
 
Descriptive Properties
ColorGrey
Mixing ratio100:12.5mixture A+B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOOLK037 / 318516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.