MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
PoolKemie POLIMOLD TR 70 Polyurethane rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Introduction: Two component room temperature vulcanizing poly-urethane rubber which cures with addition of the appropriate hardener. Once cured, this rubber becomes flexible and resistant, free from air bubbles and imperfections. It is suitable in the manufacture of moulds for production of articles made of plaster and cement thanks to its accurate reproduction of fine details and due to its extremely low linear shrinkage.

Application: POLIMOLD TR is specially suited for production of decorative plaster subjects, religious articles, statues, pottery, artistic ceramics, sanitary, precast concrete, garden ornaments, etc. Types characterized by high Shore A hardness value, are suited for reproduction of large-sized patterns.

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccmixture A+B
Viscosity 4000 cPmixture A+B
Linear Mold Shrinkage <= 0.010 cm/cmafter 5 days ageing; ISO 4823
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67 - 73
Elongation at Break >= 250 %
Tear Strength 6.00 - 8.00 kN/mDIN 53515
 
Processing PropertiesOriginal ValueComments
Cure Time 7.00 - 10.0 hourHardening time
 24.0 hourDemoulding time
Pot Life 20.0 minmixture A+B
 
Descriptive Properties
ColorGrey
Mixing ratio100:12.5mixture A+B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK037 / 318516

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.