MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum Bronze, UNS C61300, H04 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold formability. Fair to poor machinability

Applications: nuts, bolts, stringers and threaded members, corrosion resistant vessels and tanks, structural components, machine parts, condenser tube and piping systems, marine protective sheathing and fasteners, munitions mixing troughs and blending chambers.

Properties typical for 13mm thick plate .

Key Words: CDA 613
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.89 g/ccapproximately 1.8% volume contraction on freezing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 91
Tensile Strength, Ultimate 585 MPa
Tensile Strength, Yield 400 MPa
@Strain 0.5 %
Elongation at Break 35 %in 50 mm
Reduction of Area 25 %
Modulus of Elasticity 115 GPa
Compressive Strength 860 MPa
Poissons Ratio 0.312
Fatigue Strength 180 MPa
@# of Cycles 1.00e+8
Reverse Bending
Machinability 30 %Based on 100% machinability for UNS C360000
Forgeability 50 %
Shear Modulus 44.0 GPa
Izod Impact 54.0 - 66.0 J
@Temperature -30.0 - 150 °C
Temper not specified
Charpy Impact 81.0 - 88.0 J
@Temperature -30.0 - 150 °C
Keyhole; temper not reported
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.16
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.375 J/g-°C
Thermal Conductivity 56.5 W/m-K
@Temperature 20.0 °C
Melting Point 1040 - 1045 °C
Solidus 1040 °C
Liquidus 1045 °C
Annealing Point 1125 - 1600 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1010 °CHot-Shortness Temperature
Annealing Temperature 600 - 875 °C
Hot-Working Temperature 800 - 925 °C
Recrystallization Temperature 785 - 870 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.0 - 7.5 %
Copper, Cu 88.5 - 91.5 %
Iron, Fe 2.0 - 3.0 %
Lead, Pb <= 0.010 %
Manganese, Mn <= 0.10 %
Other, total <= 0.050 %
Tin, Sn 0.020 - 0.50 %
Zinc, Zn <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phosphor bronze 8% Sn, UNS C52100, H02 Temper rod
Aluminum Bronze, UNS C61300, O60 Temper
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO35 Temper rod
Aluminum Bronze D, UNS C61400, H04 Temper 25 mm flat products
Aluminum Bronze D, UNS C61400, O60 Temper 25 mm flat products

MC61300b3 / 171637

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.