MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Bronze D, UNS C61400, O60 Temper 25 mm flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold formability.

Applications: nuts, bolts, stringers and threaded members, corrosion resistant vessels and tanks, structural components, machine parts, condenser tube and piping systems, marine protective sheathing and fasteners, munitions mixing troughs and blending chambers.

Test specimen: flat products - 25 mm thickness.

Key Words: CDA 614
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 80 - 8480 - 84
Tensile Strength, Ultimate 525 MPa76100 psi
Tensile Strength, Yield 230 MPa
@Strain 0.5 %
33400 psi
@Strain 0.5 %
Elongation at Break 45 %45 %In 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Compressive Strength 825 MPa120000 psi
Poissons Ratio 0.3120.312
Fatigue Strength 180 MPa
@# of Cycles 1.00e+8
26100 psi
@# of Cycles 1.00e+8
Reverse Bending; Temper Not Reported
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 275 MPa39900 psi
Izod Impact 54.0 - 61.0 J39.8 - 45.0 ft-lbTemper not specified
Charpy Impact 81.0 - 88.0 J59.7 - 64.9 ft-lbKeyhole, temper not reported
 35.0 J
@Temperature 550 °C
25.8 ft-lb
@Temperature 1020 °F
V Notch, annealed (specific temper not reported)
 55.0 J
@Temperature 425 °C
40.6 ft-lb
@Temperature 797 °F
V Notch, annealed (specific temper not reported)
 78.0 J
@Temperature 320 °C
57.5 ft-lb
@Temperature 608 °F
V Notch, annealed (specific temper not reported)
 84.0 J
@Temperature 200 °C
62.0 ft-lb
@Temperature 392 °F
V Notch, annealed (specific temper not reported)
 85.0 J
@Temperature -175 °C
62.7 ft-lb
@Temperature -283 °F
V Notch, annealed (specific temper not reported)
 90.0 J
@Temperature 0.000 °C
66.4 ft-lb
@Temperature 32.0 °F
V Notch, annealed (specific temper not reported)
 91.0 J
@Temperature -50.0 °C
67.1 ft-lb
@Temperature -58.0 °F
V Notch, annealed (specific temper not reported)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000123 ohm-cm
@Temperature 20.0 °C
0.0000123 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 56.5 W/m-K392 BTU-in/hr-ft²-°F
Melting Point 1040 - 1045 °C1900 - 1913 °F
Solidus 1040 °C1900 °F
Liquidus 1045 °C1913 °F
Annealing Point 607.2 - 899 °C1125 - 1650 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1010 °C1850 °FHot-Shortness Temperature
Annealing Temperature 600 - 900 °C1110 - 1650 °F
Hot-Working Temperature 800 - 925 °C1470 - 1700 °F
Recrystallization Temperature 785 - 870 °C1450 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 - 8.0 %6.0 - 8.0 %
Copper, Cu 88 - 92.5 %88 - 92.5 %
Iron, Fe 1.5 - 3.5 %1.5 - 3.5 %
Lead, Pb <= 0.010 %<= 0.010 %
Manganese, Mn <= 1.0 %<= 1.0 %
Other, total <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.015 %<= 0.015 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze D, UNS C61400, H04 Temper 25 mm flat products
Aluminum Bronze, UNS C61300, O60 Temper
Aluminum Bronze, 5%, UNS C60600, H04 Temper
Aluminum Bronze, UNS C61300, H04 Temper
Aluminum Bronze, 5%, UNS C60600, O60 Temper

MC61400b6 / 11585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.