MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products BC 9020 Silicone RTV Rubber
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: BC 9020 is a violet colored, two-component, flowable compound that regardless of thickness or confinement, cures at room temperature. The cured rubber is high strength and high tear with good elongation. In addition, BC9020 features low viscosity, low durometer and resistance to sulfur clays. Application: BC 9020 is a mold making material designed for the manufacture of flexible molds. These rubber molds are recommended for the use in repetitive production of intricate shapes cast from epoxy or urethane resins. These molds are also used in the potting of electronic components and in protecting sensitive assemblies against thermal shock and vibration. Temperatures above 80º F in the modeling and encapsulating area should be avoided to prevent premature expiration of pot life. BC9020 should be thoroughly stirred before mixing, since pigments settle during storage. Mixing containers should be clean and dry before use and then should be filled to 1/4 capacity to allow room for mixing and deaeration. It is recommended that separate tools be used for mixing the catalyst and the compound to avoid cross contamination. When mixing by hand, material clinging to sides and bottom should be folded into main contents twice. When mixing is done with a power mixer, two fifteensecond cycles are generally sufficient for thorough mixing. Avoid prolonged mixing at high speeds as this will generate heat and decrease the pot life of the material. Deaeration: Air entrapped during the mixing cycle must be removed to eliminate voids in the cured compound. Place the mixture in a vacuum of 29 inches of mercury. The mixture will expand to `3-5 times its original volume, crest and recede approximately to its original level. Continue the deaeration for an additional 1-2 minutes and the material will be ready to use.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Brookfield Viscosity 10000 cPCatalyst
 3.10e+6 cPMixed
 7.00e+6 cP
@Temperature 25.0 °C
Compound
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 25
Tensile Strength, Ultimate 600 psi
Elongation at Break 500 %
Tear Strength 120 pli
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 450 °Festimate
 
Processing PropertiesOriginal ValueComments
Cure Time 480 min
@Temperature 24.0 °C
handling time
 1440 min
@Temperature 24.0 °C
90% cure
 2880 min
@Temperature 24.0 °C
full cure
Pot Life 60 min
@Temperature 25.0 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Mix Ratio10:1 by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products BC 8860 Polyurethane Elastomer
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane
Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber
Humiseal 1C49 Silicone Conformal Coating
Humiseal 1C51 Silicone Conformal Coating

PBCC058 / 107285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.