MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Esstech V-117-1140 Barium Borosilicate Glass
Categories: Ceramic; Glass; Glass Ceramic; Oxide; Silicon Oxide

Material Notes: Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of particle sizes. CAS # 65997-17-4.

Information provided by ESSTECH, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.049 g/cc
Particle Size 14 µmmedian
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.625 µm/m-°C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.553
 
Component Elements PropertiesOriginal ValueComments
B2O3 9.0 %
BaO 33 %
SiO2 50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Celanese Fortron® 1140 A0 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)

PESST004 / 108275

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.