MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinability

Characteristics: Excellent machinability compared to Formadur® 2311

Applications: Injection molds where surface finish is not critical, Mold bases, Die holders, Ejector plates and Rubber mold

Information provided by Schmolz + Bickenbach

Key Words: DIN 1.2312
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C  28
@Treatment Temp. 700.0 °C,
Time 7200 sec
28
@Treatment Temp. 1292 °F,
Time 2.00 hour
 36
@Treatment Temp. 600.0 °C,
Time 7200 sec
36
@Treatment Temp. 1112 °F,
Time 2.00 hour
 42
@Treatment Temp. 500 °C,
Time 7200 sec
42
@Treatment Temp. 932 °F,
Time 2.00 hour
 46
@Treatment Temp. 400 °C,
Time 7200 sec
46
@Treatment Temp. 752 °F,
Time 2.00 hour
 48
@Treatment Temp. 300 °C,
Time 7200 sec
48
@Treatment Temp. 572 °F,
Time 2.00 hour
 50
@Treatment Temp. 200 °C,
Time 7200 sec
50
@Treatment Temp. 392 °F,
Time 2.00 hour
 51
@Treatment Temp. 100 °C,
Time 7200 sec
51
@Treatment Temp. 212 °F,
Time 2.00 hour
Tensile Strength 924 MPa134000 psi32 HRC
 848 MPa
@Treatment Temp. 700.0 °C
123000 psi
@Treatment Temp. 1292 °F
28 HRC
 1140 MPa
@Treatment Temp. 600.0 °C
165000 psi
@Treatment Temp. 1112 °F
36 HRC
 1330 MPa
@Treatment Temp. 500 °C
193000 psi
@Treatment Temp. 932 °F
42 HRC
 1480 MPa
@Treatment Temp. 400 °C
215000 psi
@Treatment Temp. 752 °F
46 HRC
 1570 MPa
@Treatment Temp. 300 °C
228000 psi
@Treatment Temp. 572 °F
48 HRC
 1670 MPa
@Treatment Temp. 200 °C
242000 psi
@Treatment Temp. 392 °F
50 HRC
 1730 MPa
@Treatment Temp. 100 °C
251000 psi
@Treatment Temp. 212 °F
51 HRC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.2 µm/m-°C
@Temperature 21.1 - 93.3 °C
6.80 µin/in-°F
@Temperature 70.0 - 200 °F
 13.0 µm/m-°C
@Temperature 21.1 - 204 °C
7.20 µin/in-°F
@Temperature 70.0 - 400 °F
 13.7 µm/m-°C
@Temperature 21.1 - 302 °C
7.60 µin/in-°F
@Temperature 70.0 - 575 °F
Thermal Conductivity  38.9 W/m-K
@Temperature 302 °C
270 BTU-in/hr-ft²-°F
@Temperature 575 °F
 39.8 W/m-K
@Temperature 100 °C
276 BTU-in/hr-ft²-°F
@Temperature 212 °F
 40.3 W/m-K
@Temperature 204 °C
280 BTU-in/hr-ft²-°F
@Temperature 400 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 710 - 740.6 °C1310 - 1365 °FCooling: Furnace; < 235 HB
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.40 %0.40 %
Chromium, Cr 1.9 %1.9 %
Iron, Fe 95.95 %95.95 %
Manganese, Mn 1.5 %1.5 %
Molybdenum, Mo 0.20 %0.20 %
Sulfur, S 0.050 %0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel
Schmolz + Bickenbach Formadur® 2311 (P-20 MOD.) Plastic Mold Steel
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC)
Aluminum 5083-O

NSCHMO002 / 125875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.