MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Techmer ES HiFill® PP 0123 C Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Availability: North America

Forms: Pellets

Features: Copolymer and Thermally Conductive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm
@Thickness 3.17 mm
0.0090 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7070ASTM D785
Tensile Strength, Yield 15.2 MPa2200 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Flexural Strength 20.7 MPa3000 psiASTM D790
Flexural Modulus 1.59 GPa230 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.17 mm
1.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Strength 11.8 kV/mm300 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 39.6 µm/m-°C22.0 µin/in-°FASTM D696
Thermal Conductivity 1.30 W/m-K9.00 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C175 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C125 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Imerys NYGLOS® 4W STO105 Wollastonite in Polypropylene
E-Polymers SEPAZ® LC30 PP Copolymer LFT Resin
Ensinger TECAFINE™ PP Polypropylene (PP)
Celanese SO.F.TER Technoprene® 3K3 Glass-Reinforced Polypropylene

PTPC0537 / 136475

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.