MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Imerys NYGLOS® 4W STO105 Wollastonite in Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NB

Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite an ideal performance mineral for a broad range of industrial and consumer applications.

.Information provided by NYCO Minerals, subsequently acquired by Imerys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Filler Content 15 %15 %ISO 34351
Moisture Absorption 0.00200 %0.00200 %
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inAverage
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/in
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/in
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.0 MPa2900 psi50 mm/min - CH; ISO 527
Elongation at Break 130 %130 %50 mm/min - CH; ISO 527
Flexural Strength 27.0 MPa3920 psi2 mm/min; ISO 178
Flexural Modulus 2.015 GPa292.3 ksi2 mm/min; ISO 178
Charpy Impact, Notched  0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 4.60 J/cm²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 66.0 µm/m-°C
@Temperature -30.0 - 120 °C
36.7 µin/in-°F
@Temperature -22.0 - 248 °F
ISO 11359
CTE, linear, Transverse to Flow 64.0 µm/m-°C
@Temperature -30.0 - 120 °C
35.6 µin/in-°F
@Temperature -22.0 - 248 °F
ISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene

PNYCOM90 / 150099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.