MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay LTM® 12 Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: LTM10 series tooling prepregs, including LTM® 12, are low temperature curing epoxy resins systems that can be post cured to produce tools with a service temperature of 200°C (392°F). These prepregs are suitable for the manufacture of small to large tools.

Features & Benefits:

  • 2 to 6 days out life at 21°C (70°F)
  • Minimum of 6 months storage at -18°C (0°F)
  • Autoclave cure
  • Mold tools directly from low temperature master
  • Prepregs have excellent tack and drape
  • Initial cure temperatures down to 20°C (68°F)
  • Able to produce tools with low residual stress
  • Unsupported (free standing) post-cure
  • Low tool shrinkage matched to Cytec’s tooling block expansion during cure
  • Low tooling coefficient of thermal expansion (CTE) matched with Cytec-supplied backing structures
  • Good retention of mechanical properties up to 180°C (356°F) when fully post cured
  • Long term service up to 200°C (392°F) in air
Product Variants:
LTM10: Suitable for rapid, very low temperature initial cure of smaller tools
LTM12: Suitable for low temperature initial cure of small-medium tools
LTM16: Suitable for low to medium temperature initial cure of large tools due to longer out life.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³Post cured
Storage Temperature -18.0 °C-0.400 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  2.00 - 3.00 µm/m-°C
@Temperature 21.0 - 180 °C
1.11 - 1.67 µin/in-°F
@Temperature 69.8 - 356 °F
Post cured laminated, Carbon tool
 10.5 - 12.0 µm/m-°C
@Temperature 21.0 - 180 °C
5.83 - 6.67 µin/in-°F
@Temperature 69.8 - 356 °F
Post cured laminated, glass tool
Maximum Service Temperature, Air 200 °C392 °F
Glass Transition Temp, Tg 45.0 °C113 °FCure at 30°C
 55.0 °C131 °FCure at 40°C
 65.0 °C149 °FCure at 50°C
 75.0 °C167 °FCure at 60°C
 205 - 210 °C401 - 410 °FFully post cured
Shrinkage 0.050 %0.050 %Post cured laminated, Carbon tool
 0.12 %0.12 %Post cured laminated, glass tool
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 90.0 °C
2.00 hour
@Temperature 194 °F
 180 min
@Temperature 80.0 °C
3.00 hour
@Temperature 176 °F
 600 min
@Temperature 60.0 °C
10.0 hour
@Temperature 140 °F
 1200 min
@Temperature 50.0 °C
20.0 hour
@Temperature 122 °F
 2100 min
@Temperature 40.0 °C
35.0 hour
@Temperature 104 °F
 4200 min
@Temperature 30.0 °C
70.0 hour
@Temperature 86.0 °F
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
Armstrong X-6/E Epoxy Adhesive
Hexcel® HexPly® F263 Epoxy Resin
Hexcel® HexPly® 922-1 180°C Curing Epoxy Matrix
Solvay CYCOM® 7668 Epoxy Resin

PCYTED194 / 180496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.