MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen GF 7750 M3 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Hostalen GF 7750 M3 is a high density polyethylene with medium molar mass and special narrow molar mass distribution. This grade contains a lubricant. Hostalen GF 7750 M3 is an easy flowing polymer, which shows good processing performance on monofilament production lines. Monofilaments made of Hostalen GF 7750 M3 exhibit excellent tensile properties. Typical customer applications are nets, geotextiles and protective netting in agriculture and building industry. It is used for monofilament applications requiring higher tenacity. This product is not intended for use in medical and pharmaceutical applications.

Availability: Europe

Application: Geotextile & Agriculture; Nets; Raffia/Tapes/Strapping

Market: Textile

Processing Method: Blown Film; Monofilament; Tapes & Raffia

Attribute: Copolymer; Narrow Molecular Weight Distribution

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.957 g/ccISO 1183-1
Melt Flow 0.600 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 1.70 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 18.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °CPeak; ISO 11357-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9626 / 324561

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.