Hostalen GF 7750 M3 is a high density polyethylene with medium molar mass and special narrow molar mass distribution. This grade contains a lubricant. Hostalen GF 7750 M3 is an easy flowing polymer, which shows good processing performance on monofilament production lines. Monofilaments made of Hostalen GF 7750 M3 exhibit excellent tensile properties. Typical customer applications are nets, geotextiles and protective netting in agriculture and building industry. It is used for monofilament applications requiring higher tenacity. This product is not intended for use in medical and pharmaceutical applications. Availability: Europe Application: Geotextile & Agriculture; Nets; Raffia/Tapes/Strapping Market: Textile Processing Method: Blown Film; Monofilament; Tapes & Raffia Attribute: Copolymer; Narrow Molecular Weight Distribution Information provided by LyondellBasell. |