MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Unifrax Insulfrax® Paper
Categories: Ceramic

Material Notes: Insulfrax® Paper is an evolutionary product which is manufactured by forming Insulfrax Fiber in a nonwoven matrix. These fibers are randomly oriented during manufacturing and then held in place with a latex binder system. A specialized paper-making process is utilized to form uniform lightweight, flexible materials, including Insulfrax Paper.

Insulfrax Fiber, utilized in Insulfrax Paper, in based upon a calcium, magnesium, silicate (CMS) chemistry. This CMS fiber chemistry has been successfully used to solve a variety of application problems from 800°F (427°C) up to 2012°F (1100°C). In addition to high temperature resistance, Insulfrax Fiber meets European regulatory requirements (Directive 97/69/EC).

The calcium, magnesium, silicate chemistry of Insulfrax Fiber provides superior wetting resistance to molten aluminum alloys. Testing with corrosive aluminum alloys at elevated temperatures has proven that Insulfrax is superior to traditional alumina/silica refractory ceramic fibers.

Insulfrax Paper will generate small amounts of smoke and trace element outgassing during initial exposure to temperatures above 450°F (232°C).

    Advantages
  • High-temperature stability up to 2012°F (1100°C)
  • Meets European regulatory requirements
  • Superior wetting resistance to molten aluminum
  • Low thermal conductivity
  • Flexibility
  • Easy to wrap, shape, or cut

    Applications
  • Automotive and aerospace heat shields
  • Gaskets for ovens, stoves, heaters, and other appliances
  • Nonferrous ingot mold liners
  • Refractory backup insulation in ladles, glass tanks, and other high-temperature furnaces
  • Parting medium in brazing and soldering
  • Molten aluminum transfer systems

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.144 - 0.160 g/cc0.00521 - 0.00579 lb/in³
Loss On Ignition <= 12 %<= 12 %(Wt.) including binder
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 0.248 MPa>= 36.0 psiAverage
 
Thermal PropertiesMetricEnglishComments
Melting Point 1310 °C2390 °F
Maximum Service Temperature, Air 1100 °C2010 °FRecommended Operating Temperature
Shrinkage <= 4.0 %
@Temperature 1100 °C,
Time 86400 sec
<= 4.0 %
@Temperature 2010 °F,
Time 24.0 hour
 
Descriptive Properties
ColorWhite
Fiber Index (% Wt)>50
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin POLYFLON PA-5L PTFE Paper
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
Chosun Refractories 1500 ACE PAPER Paper
Chosun Refractories 1260PAPER Paper
Overview of materials for T 300 Series Stainless Steel

CUNIF120 / 97892

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.