MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Niagara LaSalle 1212 Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel

Material Notes: This is basic screw machine steel. The grade is used as a standard of comparison for machinability (1212 is rated as 100%). It machines easily, provides good surface finish and has good brazing properties. This steel is difficult to weld and not suitable for case hardening. Generally used where mechanical properties can be sacrificed for machinability.

Information provided by Niagra LaSalle Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 167167
Tensile Strength 538 MPa78000 psi
Tensile Strength, Yield 414 MPa60000 psi
Elongation at Break >= 10 %>= 10 %2"
Reduction of Area 35 %35 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.13 %<= 0.13 %
Iron, Fe 98.52 - 99.07 %98.52 - 99.07 %as balance
Manganese, Mn 0.70 - 1.0 %0.70 - 1.0 %
Phosphorus, P 0.070 - 0.12 %0.070 - 0.12 %
Sulfur, S 0.16 - 0.23 %0.16 - 0.23 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1213 Steel, cold drawn, 19-38 mm round
Overview of materials for AISI 1000 Series Steel
AISI 1213 Steel, hot rolled, 19-38 mm round
Niagara LaSalle 1018 Cold Finished Steel Bar
AISI 1117 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

NNIAL010 / 160300

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.