This is basic screw machine steel. The grade is used as a standard of comparison for machinability (1212 is rated as 100%). It machines easily, provides good surface finish and has good brazing properties. This steel is difficult to weld and not suitable for case hardening. Generally used where mechanical properties can be sacrificed for machinability.Information provided by Niagra LaSalle Corporation |