MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Versalis Intene® C 30 AF Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Intene® C 30 AF is a solution polymerized low cis polybutadiene produced using an alkyl lithium catalyst. A TNPP free, food contact approved, non-staining antioxidant is added during the production process.

Key Features: Its unique molecular structure gives fast dissolving time and fine dispersion for the rubber in the plastic matrix.

Main Applications: Impact improver of ABS and polystyrene giving a gloss surface. It can also be used in conjunction with certain block copolymers to give high gloss. The high capacity of loading carbon black and good extrudibility make this grade suitable for abrasion strips construction in tire building.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Viscosity 42 cP
@Temperature 25.0 °C
42 cP
@Temperature 77.0 °F
of Solution, 5% wt/wt in Styrene
Mooney Viscosity 40
@Temperature 100 °C
40
@Temperature 212 °F
ASTM D1646
Ash <= 0.10 %<= 0.10 %ASTM D5667
 
Descriptive Properties
Apha Color5ASTM D1209
Cis - 1:4 Content, min38%Internal Method
Gel Rating, max5Internal Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Intene® 40 AF Butadiene Rubber
Dow Buna® SB 1500 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Overview of materials for Styrene-Butadiene Copolymer, SBC
Overview of materials for Styrene/Butadiene/Styrene (SBS)
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)

PENG202 / 124596

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.