MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reade Advanced Materials Chromium Trioxide (CrO3)
Categories: Ceramic; Oxide

Material Notes: Description: A hexavalent chromium compound and a powerful oxidizing agent. Health effects are limiting applications. Uses: Chromium plating, wood preservation industry, anodizing aluminum, corrosion resistance applications, sealing phosphate coatings applied to iron or steel, bright dipping of brass, acid cleaning of Al and Mg and organic synthesis.
Forms Available: Various granulations available from 3-6 mm fused pieces down to as small as nanoparticles.

Information provided by Reade Advanced Materials.

Key Words: CrO3, chromic acid, chromium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.70 - 5.00 g/cc2.70 - 5.00 g/ccat 20 degrees Celsius
pH 1.01.0
Molecular Weight 118.01 g/mol118.01 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1990 °C3610 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chromium (VI) Oxide, CrO3
Chromium (III) Oxide, Cr2O3 (Eskolaite)
Tungsten Carbide, W2C
Tungsten Carbide, WC
H.C. Starck Amperit® 703.053 Chromium Oxide (Cr2O3) 99.5%

CREADE004 / 1938

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.