MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
High-Leaded Tin Bronze, UNS C94300, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal and Sand.

Applications: High-speed bearings for light loads.

Classified under: High-leaded tin bronzes. ASTM B66; ASTM B584; formerly ASTM B144-3E

Typical data for sand-cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.5%

Key Words: High lead tin bronze, ASTM B66, ASTM B584, ASTM B144-3E
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.29 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 48
Tensile Strength, Ultimate 185 MPa
Tensile Strength, Yield 90.0 MPa
@Strain 0.5 %
Elongation at Break 10 %in 50 mm
Reduction of Area 8.0 %
Modulus of Elasticity 72.4 GPa
Compressive Strength 76.0 MPaat permanent set of 0.1%
 160 MPaat permanent set of 10%
Machinability 80 %UNS C36000 (free-cutting brass) = 100%
Izod Impact 7.00 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000019156 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.376 J/g-°C
Thermal Conductivity 62.7 W/m-K
@Temperature 20.0 °C
Melting Point 315 °CIncipient
 900 - 925 °C
Solidus 900 °C
Liquidus 925 °C
Shrinkage 1.1 %Patternmaker's Shrinkage (1/8 in./ft.)
 
Component Elements PropertiesOriginal ValueComments
Antimony, Sb <= 0.70 %
Copper, Cu 68.5 - 73.5 %
Iron, Fe <= 0.15 %
Lead, Pb 22 - 25 %
Nickel, Ni <= 0.70 %
Phosphorus, P <= 0.050 %
Sulfur, S <= 0.080 %
Tin, Sn 4.5 - 6.0 %
Zinc, Zn <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Leaded Phosphor Bronze, UNS C94400, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93800, Copper Casting Alloy, Centrifugally Cast
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93500, Copper Casting Alloy
Medium Bronze, UNS C94500, Copper Casting Alloy

MC94300b1 / 11955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.