MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond Ablebond 744-2NTN1 Electrically Insulating Polyimide Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS

Material Notes: Ablebond 744-2NTN1 structural epoxy adhesive is a nonsag version of 744-2 adhesive.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 24000 cP24000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Adhesive Bond Strength 17.2 MPa2500 psiLap shear, alum to alum
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
 240 min
@Temperature 75.0 °C
4.00 hour
@Temperature 167 °F
Shelf Life 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 789-4 Thermally Conductive Adhesive
Tra-Con Tra-Bond 972-1 Thermally Conductive Flexible Epoxy Adhesive
Tra-Con Tra-Bond Ablebond 933-1.5 Moisture Resistant Encapsulant
Tra-Con Tra-Bond Ablebond 862-2 Room Temperature Cure Epoxy Adhesive
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive

PTRAC150 / 71078

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.