MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals INCOLOY® alloy 908  (discontinued **)
Categories: Metal; Superalloy; Iron Base; Nickel Base

Material Notes: INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue crack growth resistance, good ductility, metallurgical stability and weldability plus sufficient resistance to stress accelerated grain boundary oxygen embrittlement (SAGBO) to permit hot fabrication without cracking. This cobalt-free, low CTE alloy was designed to meet sheathing material requirements for internally cooled Nb3Sn superconductor magnets to be used in prototype fusion reactors at cryogenic operating temperatures of -452°F (-269°C). With low temperature properties it is excellent for cryogenic applications.

Information Provided by Special Metals Corporation

Key Words: UNS N09908; ASTM B 872
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 38 - 40
Tensile Strength at Break 1172 MPa
Tensile Strength, Yield 827 MPa
@Strain 0.2 %
Elongation at Break 12 %
Modulus of Elasticity 163.3 GPa
Poissons Ratio 0.265
Shear Modulus 64.6 GPa
 
Electrical PropertiesOriginal ValueComments
Curie Temperature 282 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.59 µm/m-°C
@Temperature 93.0 °C
 8.66 µm/m-°C
@Temperature 260 °C
 11.11 µm/m-°C
@Temperature 427 °C
 12.2 µm/m-°C
@Temperature 538 °C
 13.18 µm/m-°C
@Temperature 649 °C
 14.11 µm/m-°C
@Temperature 760 °C
Specific Heat Capacity 0.439 J/g-°C
Thermal Conductivity 11.05 W/m-K
Melting Point 1361 - 1410 °C
Solidus 1361 °C
Liquidus 1410 °C
Minimum Service Temperature, Air <= -452 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.75 - 1.25 %
Boron, B <= 0.012 %
Carbon, C <= 0.030 %
Chromium, Cr 3.75 - 4.5 %
Cobalt, Co <= 0.50 %
Copper, Cu <= 0.50 %
Iron, Fe 35.588 - 44.6 %Balance
Manganese, Mn <= 1.0 %
Nickel, Ni 47 - 51 %
Niobium, Nb (Columbium, Cb) 2.7 - 3.3 %
Phosphorus, P <= 0.015 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.0050 %
Titanium, Ti 1.2 - 1.8 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 907
Special Metals INCOLOY® Alloy 909
Proto Labs Inconel 718 - DMLS
Special Metals INCOLOY® Alloy 330
Special Metals INCOLOY® Alloy 800

NINDA11 / 98902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.