MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Special Metals INCOLOY® Alloy 907
Categories: Metal; Superalloy; Iron Base

Material Notes: A nickel-iron-cobalt alloy with additions of niobium and titanium for precipitation hardening. It has the low coefficient of expansion and high strength of INCOLOY alloy 903 but with improved notch-rupture properties at elevated temperatures. Used for components of gas turbines including seals, shafts, and casings. Standard product forms are round, flats, forging stock, extruded section, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: UNS N19907
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.33 g/cc0.301 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1140 MPa
@Temperature 550 °C
165000 psi
@Temperature 1020 °F
Precipitation Hardened prior to test
 1350 MPa
@Temperature 23.0 °C
196000 psi
@Temperature 73.4 °F
Tensile Strength, Yield 1100 MPa
@Strain 0.2 %
160000 psi
@Strain 0.2 %
Precipitation Hardened. Value at room temperature
 970 MPa
@Strain 0.2 %,
Temperature 550 °C
141000 psi
@Strain 0.2 %,
Temperature 1020 °F
Precipitation Hardened prior to test
Elongation at Break 10 %10 %Precipitation Hardened
 10 %
@Temperature 550 °C
10 %
@Temperature 1020 °F
Precipitation Hardened prior to test.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000697 ohm-cm0.0000697 ohm-cm
Curie Temperature 400 - 455 °C752 - 851 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.70 µm/m-°C
@Temperature 20.0 - 427 °C
4.28 µin/in-°F
@Temperature 68.0 - 801 °F
Specific Heat Capacity 0.431 J/g-°C0.103 BTU/lb-°F
Thermal Conductivity 14.8 W/m-K103 BTU-in/hr-ft²-°F
Melting Point 1335 - 1400 °C2435 - 2550 °F
Solidus 1335 °C2435 °F
Liquidus 1400 °C2550 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.030 %0.030 %
Cobalt, Co 13 %13 %
Iron, Fe 42 %42 %
Nickel, Ni 38 %38 %
Niobium, Nb (Columbium, Cb) 4.7 %4.7 %
Silicon, Si 0.15 %0.15 %
Titanium, Ti 1.5 %1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 909
Special Metals INCOLOY® Alloy 903
Special Metals NI-SPAN-C® Alloy 902
California Fine Wire Alloy 52 Nickel Iron Alloy
Special Metals INCOLOY® alloy 908

NINC85 / 17428

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.