MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Isoflon PA 6G Cast Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes:
  • General use for mechanical parts
  • Good heat resistance
  • Easy to use
  • High moisture regain

Information provided by Isoflon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccDIN 53479
Water Absorption 2.0 %2.0 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D785
Tensile Strength 75.0 MPa10900 psiDIN 53455
Elongation at Break 60 %60 %DIN 53455
Tensile Modulus 2.40 GPa348 ksiDIN 53457
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmDIN 53482
Dielectric Constant 3.7
@Frequency 1000 Hz
3.7
@Frequency 1000 Hz
DIN 53483
Dielectric Strength 19.0 - 29.0 kV/mm483 - 737 kV/inDIN 53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.0 µm/m-°C41.7 µin/in-°FDIN 52328
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °FDIN 53736
Maximum Service Temperature, Air 100 °C212 °FContinuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °FContinuous; DIN 52612
Flammability, UL94 V-2V-2
 
Descriptive Properties
ColorNat.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling SUSTAMID® 6G PA 6G/ Cast Nylon
Akro-Plastic Akromid® A3 1 black (2417) PA 66 Dry
EPICHEM Epinyl PA 66 Polyamide 66
Domo Technyl® C216V25 25% Glass Filled Nylon 6
Plastcom SLOVAMID 66 GF 25 TS PA66, 25% glass fibre, thermal stability

PISOFL912 / 123300

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.