MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 66 GF 25 TS PA66, 25% glass fibre, thermal stability  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Features

PA 66 for injection moulding, chemically reinforced with 25 % glass fibre, heat stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and electrical industry. Can be used in environment, in which longtime heat impact of up to 200°C occurs. Decrease in tensile strength by 50 % after 5000 hours at 170°C. The heat stabilization predetermines the products to environment with longtime heat exposure, like eg. intake pipes, cylinder heads, induction coils, carrying parts in the motor fixing in the motor area. Application: hobby tools, gears, covers of electric tools, cooling water distribution in the automotive industry. Delivered in black.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³
Viscosity Measurement 0.84 - 1.220.84 - 1.22
Linear Mold Shrinkage 0.0084 cm/cm0.0084 in/in
Linear Mold Shrinkage, Transverse 0.0122 cm/cm0.0122 in/in
Melt Flow 3.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 150 MPa21800 psi
Elongation at Break 3.0 %3.0 %
Tensile Modulus 7.50 GPa1090 ksi
Flexural Strength 215 MPa31200 psi
Flexural Modulus 6.00 GPa870 ksi
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -20.0 °C
21.4 ft-lb/in²
@Temperature -4.00 °F
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.700 J/cm²
@Temperature -20.0 °C
3.33 ft-lb/in²
@Temperature -4.00 °F
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Strength 40.0 kV/mm1020 kV/in
Comparative Tracking Index 450 V450 V
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °F
Vicat Softening Point 250 °C482 °FB
Flammability, UL94 HBHB
Glow Wire Test 650 °C1200 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
Overview of materials for Nylon 66/6

PPLACO394 / 121018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.