Hifax ETA4161U P23494 J DEERE GRY fractional melt flow, medium flexural modulus, thermoplastic polyolefin (TPO) is typically used as a cap layer for interior and exterior applications that require good scratch and mar resistance and can improve stress whitening issues. This extrusion grade material exhibits enhanced melt strength for a wide thermoforming process window. Status: Commercial - Active Availability: North America Application: Industrial; Panels & Profiles Market: Automotive Processing Method: Injection Molding Information provided by LyondellBasell. |